top of page

Raw Materials | Hammadde

  • ABS (Akrilonitril Bütadien Stiren)

Op. Temp. 175-250°C - pre-drying time 2-3 Hour drying temp 80°C

  • PA 11/12 (Poliamid 11/12)

Op. Temp. 190-250°C - pre-drying time4-6 Hour drying temp 80°C

  • PC (Polikarbonat)

Op. Temp. 220-260°C - pre-drying time 2-3 Hour drying temp 120°C

  • PET (Polietilen Tereftalat)

Op. Temp. 235-260°C - pre-drying time 4-6 Hour drying temp 170°C

  • POM (Polioksimetilen)

Op. Temp. 190-210°C - pre-drying time 3 Hour drying temp 100°C

  • PPO (Polifenilen Oksit)

Op. Temp. 250-290°C - pre-drying time 2 Hour drying temp 110°C

  • PVC (Polivinil Klorür)

Op. Temp. 180-210°C - pre-drying time 1 Hour drying temp 70°C

  • TPU (Termoplastik Poliüretan)

Op. Temp. 170-230°C - pre-drying time 2-3 Hour drying temp 90-100°C

  • ASA (Akrilonitril Stiren Akrilat)

Op. Temp. 210-260°C - pre-drying time 2-4 Hour drying temp 80°C

  • PA 6 (Poliamid 6)

Op. Temp. 240-270°C pre-drying time 3-5 Hour drying temp 80°C

  • PA 6.6/6.10 (Poliamid 6.6/6.10)

Op. Temp. 260-290°C pre-drying time 3-5 Hour drying temp 80°C

  • PE (Polietilen)

Op. Temp. 130-250°C pre-drying time 1-2 Hour drying temp 90°C

  • PET-G (Polietilen Tereftalat - Gilkol)

Op. Temp. 210-260°C pre-drying time 4-6 Hour drying temp 60-70°C

  • PP (Polipropilen)

Op. Temp. 175-225°C pre-drying time 1-2 Hour drying temp 90°C

  • PPS (Polifenilen Sülfür)

Op. Temp. 300-340°C pre-drying time 3-4 Hour drying temp 140-150°C

  • SAN (Stiren Akrilonitril)

Op. Temp. 200-240°C pre-drying time 2-3 Hour drying temp 80°C

  • CA (Selüloz Asetat)

Op. Temp. 189-220°C pre-drying time 2-3 Hour drying temp 60-65°C

  • PLA (Polilaktik Asit)

Op. Temp. 180-240°C pre-drying time 4-5 Hour drying temp 70-80°C

  • PPA (Poliftalamid)

Op. Temp. 300-330°C pre-drying time 6 Hour drying temp 80°C

  • PS (Polistiren)

Op. Temp. 210-250°C pre-drying time 1-2 Hour drying temp 80°C

  • SB (Stiren-bütadien)

Op. Temp. 130-160°C pre-drying time 1-2 Hour drying temp 80°C

  • PBT (Polibütilen Tereftalat)

Op. Temp. 240-260°C pre-drying time 4 Hour drying temp 120-140°C

  • PEI (Polieterimid)

Op. Temp. 370-390°C pre-drying time 3-4 Hour drying temp 150°C

  • PMMA (Polimetil Metakrilat)

Op. Temp. 200-270°C pre-drying time 3 Hour drying temp 80-100°C

  • PPE (Polifenilen Eter)

Op. Temp. 280-300°C pre-drying time 3-4 Hour drying temp 110-120°C

  • PSU (Polisülfon)

Op. Temp. 330-370°C pre-drying time 2-3 Hour drying temp 120-135°C

  • TPE (Termoplastik Elastomer)

Op. Temp. 120-230°C pre-drying time 2-3 Hour drying temp 110°C

bottom of page